Spare Gasket (Sealing, Dichtung) for Thomas Central Vacuum
Obliczymy ostateczną cenę na podstawie wybranego pliku. Sprawdzisz ją i zaakceptujesz przed płatnością.
Zapisane na tym urządzeniu.
After my sealings needed to be replaced I bought original sealings, which consisted of a simple foampad of about 2-3mm…
- Ocena
- 0 / 5
- Polubienia
- 1
- Pobrania
- 10
- Wydruki
- 0
- Wyświetlenia
- 246
- Oceny
- 0
Aktualizacja u źródła:
Informacje o modelu
- Źródło
- Printables
- Kategoria
- Other House Equipment
- Licencja
- Creative Commons — Attribution — Noncommercial — Share Alike
After my sealings needed to be replaced I bought original sealings, which consisted of a simple foampad of about 2-3mm thickness. Now this is very simple and cheap material for 3EUR per piece.
I had cleaned the surface of the ABS lid in order to receive a good and durable tack, but already after few times in use tese pads released from the ABS lid, so my vacuum system with 5 attaching points got untight more and more, the vacuum effectiveness behaved the same, got really worse. All substitutes I treid out were not the solution.
Now I designed a pad and printed it with my Elegoo Mars 2 Pro. Material Monocure Flex (100%). After few adaptions I think I got the right dimensions. Thickness I needed to play with.Now set to 2.4mm and I glued the part in with some far-east mobile repair glue with the expectation it stays innplay for longer than the previous mentioned org. parts. After glueing I pressed the sandwich moderately with two fitting pieces of wood, in order to get a nice tack. My today's impression is that it works. At least the sealings in place work.
I do not hear whistling noises like before, by far NOT! Which is good. Hope it will still be good in couple years?
Explore my other Printables: https://www.printables.com/de/@Tritschi
Print Settings
Printer:
Elegoo Mars 2 Pro
Rafts:
No
Supports:
No
Resolution:
0.05mm
Infill:
100%
Filament:
Monocure Resin Flex Resin
translucent
Notes:
The Elegoo Mars 2 Pro has a 4K monochrome display, Therefore exposure times are less than color displays.
I used 4 bottom layers per each 15 seconds.
The rest I exposured with 5.5 seconds.
I use a WhamBam flexible build plate. After cleaning in IPA I let it dry by blowing contant air for about 15 minutes. While the part was still on the plate I put it into a sealed plastic zipper bag and let it stay for about 20 minutes in the freezer. Then took it out and bent the WhamBam a bit, part became immediately loose, then I dried again for couple minutes unless I cured it in my Elegoo Mercury Wash & Cure for 3 minutes. End result of part is excellent!
Category: Household