Ironing Test Square 40×40×3 mm — PLA & PETG Starting Settings — image 1

Ironing Test Square 40×40×3 mm — PLA & PETG Starting Settings

Order a print of this model

We calculate the final price from your selected file. You review and accept it before payment.

Saved on this device.

An ironing testing square with some recommended settings to start your calibration.

Rating
0 / 5
Likes
1
Downloads
22
Makes
0
Views
76
Reviews
0

Updated at source:

Model information

Category
Test Models
License
Creative Commons — Attribution

## Ironing Test Square (40 × 40 × 3 mm)

A small, solid square for tuning ironing so top surfaces come out smooth instead of lined, gappy, or blobbed.

Size is large enough to see stripes and edge buildup, small enough that a test print is cheap and fast.

### Model

- 40 mm × 40 mm × 3 mm

- Solid — infill does not matter

- No supports, brim, or raft needed if your first layer is dialed in

- Designed for a 0.4 mm nozzle (works with others; adjust spacing)

### How to use

1. Slice one square with ironing on.

2. Start with the PLA or PETG values below.

3. Print. Check the top under raking light and by fingertip.

4. Change one setting at a time:

- Gaps / visible lines → raise ironing flow 2% or tighten line spacing

- Blobs, ridges, dragged lumps → drop flow 2–3% and/or raise speed a little

5. Optional: put 3–4 copies on one plate and use per-object ironing flow (8 / 10 / 12 / 14%) to pick a winner in one print.

Calibrate normal flow / extrusion multiplier first. Ironing multiplies whatever your base flow already is.

### Recommended ironing starting points (0.4 mm nozzle)

Both materials

- Ironing type: Topmost surface only (not all solid layers)

- Pattern: Rectilinear

- Ironing angle: -1 (auto) or 45°

- Inset: ~0.2 mm

- Top solid layers: 4–5 so you are not ironing over infill

PLA

| Setting | Start here | Typical range |

|---|---|---|

| Ironing flow | 10–12% | 8–15% |

| Ironing speed | 20–40 mm/s | 15–50 mm/s |

| Line spacing | 0.10–0.15 mm | 0.10–0.21 mm |

PETG

| Setting | Start here | Typical range |

|---|---|---|

| Ironing flow | 6–10% | 5–12% |

| Ironing speed | 15–30 mm/s | 15–50 mm/s |

| Line spacing | 0.12–0.21 mm | 0.10–0.21 mm |

PETG wants less flow than PLA. Too much flow leaves sticky blobs that the nozzle drags across the face.

A  start that works for a lot of people:

- Rectilinear

- 40–50 mm/s

- 10% flow

- 0.21 mm spacing

- Then drop flow if you are on PETG

### Suggested print settings (the square itself)

- Layer height: 0.16 or 0.20 mm

- Walls: 2–3

- Top/bottom: 4–5 (or 100% solid)

- Nozzle: 0.4 mm

- First layer: your normal first-layer settings

- Fan: PLA 100% after layer 1 · PETG 30–50%

- Supports / brim: off

### How to judge the winner

- Good: even satin/matte face, no stripes, no lumps, edges not piled up

- Under-extruded ironing: faint lines or tiny gaps

- Over-extruded ironing: shiny ridges, blobs, “comb” at the edges

Write the winning flow / speed / spacing on the bottom with a marker so you have a coupon for that filament.

### Notes

Different brands and colors need their own pass. White PETG and silk PLA especially drift from generic numbers.

If this helped, post a make with filament brand + the settings that won.