Low-melting-point alloy Casting: DIY Metal Dice Mold (Easy)
We calculate the final price from your selected file. You review and accept it before payment.
Saved on this device.
No furnace or fire required. This 3D printed PETG mold is designed for low-melting-point alloys (<100°C).
- Rating
- 0 / 5
- Likes
- 45
- Downloads
- 56
- Makes
- 0
- Views
- 1,055
- Reviews
- 0
Updated at source:
Model information
- Source
- Printables
- Category
- Other Toys & Games
- License
- Creative Commons — Attribution — Noncommercial
Cast real metal dice safely at home using just hot water!
This project uses a 3D printed PETG mold to cast ultra-low melting point alloys (melting point < 80°C / 176°F) without needing a furnace or open flame.
Unlike traditional casting, this method uses a hot water bath to melt the metal. Since boiling water never exceeds 100°C, you cannot accidentally overheat the metal and destroy your PETG mold.
Key Features
Real Weight: Creates solid metal dice, not plastic.
Non-Toxic & Safe: Designed for Lead-Free alloys melted in hot water.
High Detail: Optimized for 0.1mm layer height printing.
⚠ Required Materials
Low Melting Point Alloy(Lead-Free & Cadmium-Free):
Quantity: Approx. 50g - 60g per dice.
Melting Point: Must be below 100°C (e.g., 70°C - 80°C).
Reference: I used a low-melting alloy from a Japanese supplier (Link below), but any generic "Field's Metal" or "Low Temp Casting Alloy" works.
Product Link (Reference): https://www.zairyo-ya.com/?pid=178248785
PTFE-based Lubricant: (Spray or liquid) - Essential for release.
Rubber Bands: To secure the mold halves together.
Filament:PETG, ABS or ASA. PLA is NOT recommended as it will warp.
Print Settings (Crucial for Success)
To ensure the mold withstands the heat and produces a smooth finish:
Material: PETG (Required).
Layer Height: 0.1mm (Highly recommended to minimize layer lines on the casted metal).
Infill: 40% or higher (Provides structural integrity and heat absorption).
Perimeters (Walls): 3 loops or more (Ensures the mold is watertight and durable).
Supports: No supports required for the mold interior.
Casting Instructions (The Hot Water Method)
Apply Release Agent:
Apply a thin, even coat of PTFE-based lubricant to the inside of the mold parts. This prevents the metal from sticking to the PETG.
Assemble & Secure:
Close the mold parts together and wrap rubber bands tightly around them.
Tip: Ensure the mold is tightly closed to prevent molten metal from leaking out.
Melt the Alloy:
Place your Lead-Free alloy in a small metal cup. Submerge it in a bowl of hot water (approx. 90-100°C). The metal will liquify within minutes.
Pour:
Remove the container from the water and dry it off. Pour the liquid metal slowly into the mold.
Safety: Wear heat-resistant gloves (Rubber or Silicone)! The metal and water are hot enough to cause burns.
Cool Completely (CRITICAL):
Let the mold cool down completely. DO NOT open the mold while it is still warm.
Pour the liquid metal slowly into the mold.⚠ DANGER: If you open the mold before the metal has fully solidified, molten metal can splash out and cause severe burns. Be patient.
Demold & Finish:
Remove the rubber bands and release the die. Cut off the sprue and trim any flash. Sand or polish the faces if necessary.